Problems in autophoretic paint sticking on chrome plated surface




2005

Sir,

we have an problem in problems in Autophoretic paint sticking on chrome plated surface.What is the reason behind it. Our customer says that Autophoretic paint should not be stick on chrome plated surface.So please send solution on urgent basis.

With regards,

Amit Mishra
- Gurgaon, INDIA


The way I understand it, autophoretic coating should not stick to chrome plating because of the lack of Fe, however suppliers of autophoretic products have told me that not all chrome plating is alike and it must be a high quality finish (no Fe for the reaction to bond with).

Jim Johnson
- Winnipeg, Manitoba, Canada
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"