Hi,

We are looking for a way to coat small stainless steel tools and parts with different colours such as rainbow, black, purple, blue etc. Does anyone know a low cost method or machine that produces good results?

Your help is greatly appreciated.

FRANK SCHMIDT
MANUFACTURING - Dallas, Texas



Talk to Balzers, they are probably the world's top vacuum deposition company and they have a huge range of systems that give a miriade of colours. They have an internet site.

trevor crichton
Trevor Crichton
R&D practical scientist
Chesham, Bucks, UK
2005



Isoflux is another alternative. They make smaller tool coaters.

John Davis
John Davis
- Berthoud, Colorado, USA
2005


adv.
b&m finishers banner



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"