Aluminum in Clean Rooms
Is there a recommended coating for aluminum surfaces in clean rooms? What's the impact of not coating?
Donald Brunk
DuPont - Wilmington, DE, USA
2005
A simple clear anodize should do.
Tim McKenna
Semiconductor fab - Carrollton, Texas
2005
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.