mobile?
Metal finishing Q&As since 1989
-----
Gun Barrel Finish
Arch. has requested this finish on a stair stringer.
Jack Hubshman
- Dunmore, Pennsylvania
2005
The finish is black oxide. It will need a topcoat of wax or lacquer to have any reasonable corrosion resistance.
Jeffrey Holmes, CEF
Spartanburg, South Carolina
2005
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.