Stripping platinum from titanium




2005


We are the manufacturer of platinum plated titanium and niobium anodes in India. We also do refurbishment of old anodes for our customers. During the refurbishment, we would like to strip the existing platinum before replating of platinum. Is it any method for strip the existing pt. Awaiting to receive your suggestion.

Regards,

M.P.V. Jeyakumar
- Chennai, Tamil Nadu, India



We are the manufacturer of Imitation jewelry. We are using platinised titanium anodes for gold and palladium.We want to know how we can strip the platinum from the titanium anodes to re use for platinum coating on same.please suggest how to coat platinum on same.

quadri
Syed Farooq Quadri
mfgr. of costume jewelry- Hyderabad, Andhra Pradesh, India
2005


Normally, a 50:50 solution of HCl and water in a stainless steel tank with a heating element capable of heating the solution to 40-45 C would be sufficient to remove the platinum coating.

Cory Rea
- Cork, Ireland
2005


none
finishing.com is made possible by ...

this text gets replaced with bannerText
spacer gets replaced with bannerImages



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"