Electrically conductive hydrophilic coating for stainless?




I am looking for a hydrophilic coating that can be applied to 304 stainless and is electrically conductive. The coating must also be biocompatible. Is a product/process for this available?

Thanks,

Art Zikorus
medical - San Jose, California, USA
2004


Biocompatible with what? Electroless nickel might do what you are talking about, but some people are allergic to nickel if you are talking about human biocompatibility.

James Watts
- Navarre, Florida
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"