Adhesion testing of printed characters on anodize




With regards to ASTM D3363 Pencil Test. Is that test valid for testing adhesion of characters pad printed on an anodized metal surface? My impression is that the test is for a smooth painted surface only.

If there is a more preferred method for testing adhesion of characters printed on a surface, I'm all ears.

Thanks,

Bill Nibley
Manufacturing - Simi Valley, California, USA
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"