Metal finishing Q&As since 1989

-----

Color etchant for monel





I did a lot of search on "color etchant" for nickel and copper in monel but I couldn't find any one. If anybody knows please help me

mazhar I [last name deleted for privacy by Editor]
student -islamabad, Pakistan
2004



April 5, 2008

Hi, Mazhar. Sorry that I know nothing about this subject but -- according to info.lu.farmingdale.edu/~ibrahiaz/MET205/Buehler/etching.pdf -- Carapella's etch, which is 5 g FeCl, 2 ml HCl, and 99 ml ethanol is suitable for monel. Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"