Electropolishing of copper aluminium alloys





hi, I am in 4th year chemical engineering and my project is ELECTROPOLISHING OF COPPER ALUMINIUM ALLOYS USING PHOSPHORIC ACID , and I wanna know more about it and how it works!

maha farah
chemical engineer - alex, alexandria, egypt
2004



I am doing my last year in engineering metallurgy and am doing a project on electropolishing of copper. I would like to know more about the project as I'm having insufficient information. It would indeed be a privilege to hear about your input.

Thank you.

Ntobeko
- Johannesburg, South Africa
2004



April , 2008

Hi, folks. There is at least some information about electropolishing of copper in the Electroplating Engineering Handbook [on AbeBooks or eBay or Amazon (adv.)] . Good luck.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"