Electroplating of Titanium




2004

Dear Sir,

I am a student working on Biomaterials, particularly Titanium. I would like to know what other metals can be electroplated on Titanium and whether titanium could be electroplated on some other metal? Please could you suggest some literature where I could get more information on the subject.

Thanking You,

Sonia Samuel
student - Calicut, Kerala, India



Try to find Ukrainian(ex USSR) book L.I. Kadaner: Galvanostegija (Kiev 1964).In this book you can find small chapter on titanium plating.According to it you can plate titanium on Zn and Al.

Hope it helps!

Goran Budija
- Cerovski vrh Croatia
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"