Silver bracelets are yellow



Dear sirs,

We are producing a batch of pearls with silver bracelets. However, the silver becomes oxidization, the color has been changed to yellow. Of course none can accept this kind quality. Please let us know any idea / solution base on this situation. Thanks a lot!

Venus Li
Jewellery mfgr - Tsim Sha Tsui, Hong Kong, China
2004



Venus

Please find a good Silver anti tarnish and use it over the bracelets. Or use a clear lacquer. Both can help improve tarnish resistance.

Regards

asif_nurie
Asif Nurie [deceased]
- New Delhi, India
With deep regret we sadly advise that Asif passed away on Jan 24, 2016

2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"