Seeking polishing of stainless steel




I produce hydraulic steering systems for high performance boats. The mounting brackets are made from 316 stainless steel plate 3/8" thick. the largest piece is shaped like a "U" which is approximately 9" x 10". There are 10 other pieces to this bracket that range in size from 2" x 3.5" to 1" x 2". All of these have the #1 mill finish; I am looking for someone to get these to a #8 mirror finish for a reasonable price.

John Richardson
Marine accessory manufacturer - Norfolk, VA, United States
2004



I have some stainless steel brackets the largest of which is 9.5" x 9". I am interested in having them electro polished. I will need to know what the initial finish will need to be before they go in the tank. (Will the gentleman from Raleigh who responded to my post last week about polishing stainless steel please give me me a call. Unfortunately, I misplaced your number)

Thanks,

John Richardson
Marine accessory manufacturer - Norfolk, Virginia
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"