Polishing material




I'm refining precious metal from jewelry polishing dusts. After separating precious metal out, I will get lots of polishing material remain. My question is what business can make use of this material. The composition of this powder is SiO2 80-85%, Al2O3 10-15%, Iron Oxide ~2-5%.

DOME ROOKDOK
recycle business - JATUJAK, BANGKOK, THAILAND
2004



I applaud that you want to recycle this, but I would be surprised to hear that a used, mixed, abrasive is of any value at all.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2004


Could anyone in this recycle polishing dust tell me what would you do with used abrasive coming from polishing dust? Since we have lots of this used material, any use for other application or just dump it?

Dome Rookdok
recycle business - Bangkok, Thailand
2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"