Non tarnish brass alloy?




2004

Hi,

We are manufacturers of artificial jewelry. For a long time now we have been looking for a chemical coating that would give our gold n silver plated jewelry a long life.but we have been unsuccessful. Is there a chemical coating that would keep our products from getting tarnished? do you know where we can buy NON TARNISHABLE BRASS ALLOY OR METAL?

Kindly help us.

KEYUR BARAD
mgfr. of artificial jewelry - MUMBAI, MAHARASHTRA, INDIA



2004

Mr Keyur Barad,

There are a number of very good Anti tarnish treatments locally available.

1) Silver Anti tarnish
2) Gold anti tarnish
3) Clear Electrophoretic lacquer

Regards,

asif_nurie
Asif Nurie [deceased]
- New Delhi, India
With deep regret we sadly advise that Asif passed away on Jan 24, 2016



You can use aluminum bronze(copper+5-8%Al). It is very resistant to corrosion.

Goran Budija
- Cerovski vrh Croatia
2004


adv. saify ind youtube



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"