Effluent treatment of plating waste




2004

Dear Sir,

I am Shyam Sundar doing final year B.S in chemical and electrochemical engineering in India. As part of undergraduate career, I have to submit a thesis on effluent treatment of plating waste. Still now I didn't find any optimal method because I have to put material balance, energy balance, design of equipment, plant layout, cost and economics, etc., I will be very grateful to you if you could help me in this case.

Sincerely,

Shyam Sundar Venkataraman
student - Karaikudi, Tamilnadu, India


Mr Venkatraman,

Please contact the Central Pollution Control Board, New Delhi. They have a library and a number of publications that will help. Dr Jindal is the person to connect with.

Regards,

asif_nurie
Asif Nurie [deceased]
- New Delhi, India
With deep regret we sadly advise that Asif passed away on Jan 24, 2016

2004




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"