I need some color on stainless




I would like to reach some kind of information about the stainless steel coloring process (books, websites). Our shop does a lot of stainless steel polishing.

Clayton Pierce
Shop Foreman - Seattle, Washington, United States
2003


That is a very limited process and is proprietary with limited colors. There are some other possibilities, but you have not provided anywhere enough information about your product or exactly what you want it to do to have anyone be able to help.

James Watts
- Navarre, Florida
2004



You can find some information in Fishlock's book Metal Colouring!

Goran Budija
- Cerovski vrh Croatia
2004

----
Ed. note: finishing.com's supporting advertisers B&M Finishers / Prismatic Stainless Steel [a finishing.com supporting advertiser] and Russamer Labs offer coloring processes for stainless steel and may be able to help you.

adv.
b&m finishers banner



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"