Need Invar 36 with better Temperal Stability




Is there a recognised specification for Invar which will give a product that gives temperal stability better than 2 ppm per year after heat treatment? Is there anyone who stocks and/or supplies this grade of Invar?

Julie Everett
Satellite manufacture - Chilsehurst, Kent, UK
2003



Sorry, Julie: I, for one, don't understand the question. Hopefully another reader will.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2003



There is a non-commercial article that might be of use to you, at the internet (not web) address http://crswnew.cartech.com/wnew/TechArticles/TA00011.html

Bill Reynolds
Bill Reynolds [deceased]
consultant metallurgist - Ballarat, Victoria, Australia
We sadly relate the news that Bill passed away on Jan. 29, 2010.

2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"