Titration process for ABF




At present we are using Ammonium bifluoride with water for matte finish now we want analyse the chemical means titration of solution and finding out the percentage of Ammonium Bifluoride can any one help me and give titration process for this.

Thanks in advance.

Satish
Ashapura Chemicals - Ahmedabad, Gujarat, India
2003


Take a look at letter 22907 and then do a search of all the letters using the search engine. You will find several letters. Now, no one can help you until you tell us the rest of the story. What are you etching? Do you intend to analyze before use, or after use. Before is dirt simple and after use requires a lot more attention to detail. Is there any other acid in this mixture.

James Watts
- Navarre, Florida
2003


Thanks Mr James please note that we use this solution means water with 100 Gms per litr of ABF for matte finish on aluminum we want titrate the solution before & after use. Please can you help in this ?

Satish
Ashapura Chemicals - Ahmedabad, Gujarat, India
2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"