Metal finishing Q&As since 1989

-----

Cost, methods, and machinery for silver refining




RFQ: Respected sir,

I have a silver retail shop in India, in state Tamilnadu, in city Vellore. I also have an idea to open a silver bullion refinery shop. So I want the latest machinery to refine impure silver into pure silver e.g., copper with silver mixing ornaments.

Will take process into pure silver by using the latest refining machineries in many tons, please make a silver refining machinery for us. Before this please send the quotation of this machine. If it is not possible for you, please send another company's address who are able to make it or have the machinery at spot.

Please send the above details to my email address as soon as possible.

Thanking you, your's truly

t. saravana m [last name deleted for privacy by Editor]
- vellore, Tamilnadu, India
2003

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




RFQ: HELLO SIR,

I am dealing with silver production, So I want the latest machinery to refine the impure silver into pure silver.

Will take process into pure silver by using the latest refining machineries in many tons; please make the silver refining machineries for us. Before this please send the quotation of this machine. Or, please send the other companies address who can make it or have the machinery at hand.

Please send the above details to my email ASAP.

Regards,

Ahamed Hussain
silver shop - Salem, Tamil Nadu, India
2003

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




RFQ: I need information on silver refinery machinery too, give me a hand!

Alex [last name deleted for privacy by Editor]
- Shanghai, China
2006

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




RFQ: Dear sir,

I want to refine silver jewelry which contains copper, zinc, and cadmium. I want a plant eco friendly which can fulfill my requirements, and the price also. Thanking you.

ANSHUL SURANA
manufacturer silver wire - AGRA, U.P, INDIA
2004

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




Silver Recovery Techniques



(affil links)

RFQ: I want a silver refining machine.

madhur bansal
silver jewellery - agra,u.p, India
August 19, 2012


----
Ed. note: These RFQs have become outdated. To view the current RFQs or to post your own RFQ, please go to our RFQ "Hotline letters page".




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"