Need Infrared clear coatings




I too need a clear Infrared coating or spray that blocks or reflects 800-900nm I/R light off of the surface of a large plastic window. Sorry but my contract will not allow me to disclose the exact purpose of what I am doing. I will say it is very important to me and the project.

Sincerely,

John B Elliott
- Bakersfield, California, USA
2003

Ed. note: Sorry, this RFQ is old & outdated, so contact info is no longer available. However, if you feel that something technical should be said in reply, please post it; no public commercial suggestions please ( huh? why?)




Hello, John. Your question is just fine! We don't want people to spill State secrets to the world :-)

When we ask people to post their "real world situation" we want to know whether they need to have a coating applied, apply a coating themselves, formulate a coating, or answer a school homework question. We want sufficient details to be able to help them. Finally, we want enough info posted that the problem is interesting to the readers, and implies a sense of sharing and camaraderie, rather than a sense of wholesale technology transfer to the most selfish :-)

Hopefully one of our supporting advertisers will offer you a product in private, or a reader will steer you in the right direction.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2003




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"