How to strip nickel/gold coating on glass fiber
Q. I am looking for a way to remove gold/nickel metal coated on silica fiber surface, by doing so it shall not alter the properties of the glass surface, suggest me for the same.
Karthik Ram
- India
2003
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.