mobile?
Metal finishing Q&As since 1989
-----
Are these following finishes conductive?
I need to determine whether a ground path for a series of materials exists. Are the following finishes considered to be electrically conductive:
Alodine 1200
Clear Alodine
Passivated 304 stainless
Ron Kolarovic
- Hatboro, Pennsylvania, USA
2002
Yes to all 3.
Marc Green
anodizer - Boise, Idaho
2002
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.