Glass coatings colors




Dear Sir,

I am an artist. I am working glass and I want to make some colors at the surface. I want to do these coatings by spray below 650 °C. Have you some informations to produce red coatings, blue coatings, black coatings and white coatings? Thank you very much.

Sophie Labatut
- Paris, FRANCE
 


Why don't you try simply using spray paint and some sort of stencil? What kind of requirements do you have? Are you looking for coloring you can see through similar to stained glass?

tim neveau
Tim Neveau
Rochester Hills, Michigan
 

Why don't you experiment with colored vitreous enamels, rather than attempting a top color. Go to the www.thompsonenamel.com website for more info.

George Brackett III
- Utica, New York
 

Please check www.glasskote.com website. It may be of interest to you. The coating involved here is now being used widely around the world. It does not require any baking at all. Thank you Steven

Steven Vas
Euroglaze (aust) pty ltd - Australia
 



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"