Where to find Aluminum Blue 2LW Dye




I am in the process of testing per ASTM B136 (Dye Stain Test) which requires the use of aluminum blue 2LW dye. The ASTM spec offers a footnote referencing a supplier as a source for this chemical that is no longer in business.

Does any one have a current source for chemical?

Stephen Keller
- Hunt Valley, Maryland


With all of the consolidations in the metal finishing businesses, it is very hard to keep up with. That dye is manufactured by Clariant Corp in Charlotte, NC. This dye likes to mold as bad as coffee does, so do not make up any more than you can use in a week or so, or keep it in the refrigerator.

James Watts
- Navarre, Florida
 



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"