Soldering with chrome barrier metal
I have an application whereas I am am buying sapphire with a chrome underlayer and gold on top, I need to be able to then solder using 80/20 Au/Sn to a gold surface. Can this be done?
Reed Schleyer
- Hawthorne, California, USA
2001
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.