Producing Photo Resist PCB's





2001

Dear sirs,

It seems, from this page, that is possible to produce photo resist printed circuit boards, using a regular PCB and applying a dry-film or a specific type of liquid. I'd like to know from anyone informations about both processes and suppliers where I could buy the necessary material.

Thank you very much

Marco Brandao
- Porto Alegre, RS, Brazil


The easiest method is using the Press-n-Peel dry transfer system. See;

www.techniks.com/press-n-peel.html [Ed. note 11/27/06: this link is apparently no longer functional]

This does require a decent laser printer to image your layout.

Daniel Marks
- Glendale, Arizona, USA
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"