I'm having some problems with the finish on parts currently being anodized. The material is Precision Cast Tool and Jig (MIC-6). The question: Is it possible to get different colors of clear anodized parts from the same piece of material? I'm talking about night and day between the parts.

Joe Roberts
- The Woodlands, Texas
2001



I can answer your question with just one word....YES

Marc Green
Marc Green
anodizer - Boise, Idaho
2001




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"