TiN coating for 300-grade Maraging Steel?




Q. I have a highly stressed part that is steel, maraging per MIL-S-46850, type 3, grade 300.
Is Titanium Nitride a good finish to use on this material?

Arthur O'Donnell
- Gilbert, Arizona, US
August 29, 2012


A. Why do you want to deposit TiN on the maraging steel?

jim treglio portrait
Jim Treglio - scwineryreview.com
PVD Consultant & Wine Lover - San Diego,
California

August 31, 2012



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"