Formulation of Nickel plating SAE-AMS QQ-N-290 CLASS 1, GRADE F





We hope to get the exact contents for Nickel plate SAE-AMSQQN290, CLASS 1, GRADE F. Hope the experienced people can give the instructions that how we can get it, or offer the exact contents. With many thanks.

SUSAN ZHANG
precision machine production mfgr - SUZHOU, JIANG SU PROVINCE
2004



2004

Processes that comply with this spec can be purchased from CST-Surtec, Atotech, Accu-Labs, Inc. [a finishing.com supporting advertiser], EPI / Electrochemical Products Inc. [a finishing.com supporting advertiser], Macdermid, and others. Hope this helps.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"