Military Specification QQ-N-290 class 1 for screw



 

Please let me know the requirement of Military Specification FED-QQN-290 (replaced by AMSQQN290) Class 1 for screw.

Thanks,

Henry
- China, Hong Kong


A. Hello Henry!

To get a copy of any US military or federal specification, such as QQ-N-290, go to: astimage.daps.dla.mil/quicksearch/ and type the appropriate number in the document ID box.

Good luck!

lee gearhart
Lee Gearhart
metallurgist - E. Aurora, New York


----
Ed. note 5/23/13: Make that quicksearch.dla.mil/


A. QQ-N-290 is the US Federal Specification for electrodeposited nickel. Class 1 is for corrosion protection but you will need to read the entire specification to understand the requirements.

Neil Bell
Red Sky Plating
supporting advertiser
Albuquerque, New Mexico
redsky
 



(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"